Product Name : Hot Press for Plywood
Hits : 1110
Request : 0
Information : After cold pressing and repairing process, the treated basic plywood will be sent to basic plywood hot press. It will take 5-60 minutes depends on board thickness. After hot pressing, the workers will do the second time defects repairing. The board will be stored in semi product storage hours for cooling and storage. The working condition of the hot press is directly related to the production quality of the plywood, so it is especially important